" If the percentage of elongation of any tension test specimen is less than that specified in Sec. 8(a) and any part of the fracture is outside the middle third of the gage length, as indicated by scribe scratches marked on the specimen before testing,... "
Handbook of Building Construction: Data for Architects, Designing and ... - Página 1398
editado por - 1920
Visualização integral - Acerca deste livro

Bulletin, Volume 19,Parte 1

American Society for Testing Materials - 1919 - 830 páginas
...percentage of elongation of any tension test specimen is less than that specified in Section 6 (a) and any part of the fracture is outside the middle...scratches marked on the specimen before testing, a re test shall be allowed. IV. PERMISSIBLE VARIATIONS IN WEIGHT AND THICKNESS. Permissible 12. The thickness...
Visualização integral - Acerca deste livro

Book of A.S.T.M. Tentative Standards

American Society for Testing Materials - 1924 - 840 páginas
...any tension test specimen is less than that specified in Section 6 (a) and any part of the fracture b outside the middle third of the gage length, as indicated...specimen before testing, a retest shall be allowed. IV. PERMISSIBLE VARIATIONS IN WEIGHT AND THICKNESS. 11. The thickness of each plate shall not vary...
Visualização integral - Acerca deste livro

Book of A.S.T.M. Standards

American Society for Testing and Materials - 1916 - 778 páginas
...percentage of elongation of any tension test specimen is less than that specified in Section 6 (a) and any part of the fracture is outside the middle...indicated by scribe scratches marked on the specimen beforg testing, a retest shall be allowed. IV. PERMISSIBLE VARIATIONS IN WEIGHT AND THICKNESS. 11.....
Visualização integral - Acerca deste livro

Proceedings of the Annual Convention of the American Railway ..., Volume 21

American Railway Engineering Association - 1920 - 1492 páginas
...percentage of elongation of any tension test specimen is 'C5s than that specified in Section 7 (a), and any part of the fracture is outside the middle...the gage length, as indicated by scribe scratches Narked on the specimen before testing, a retest shall be allowed. (IV) Permissible Variations in Weight...
Visualização integral - Acerca deste livro

Proceedings of the Annual Convention of the American Railway ..., Volume 19

American Railway Engineering Association - 1918 - 1698 páginas
...that specified in Section 13 (c) and any part of the fracture is more than y\ inch from the center of the gage length, as indicated by scribe scratches...specimen before testing, a retest shall be allowed. Requenchlng. 15. If the results of the physical tests of any test lot do not conform to the requirements...
Visualização integral - Acerca deste livro

Proceedings of the ... Annual Convention of the American Railway ..., Volume 19

American Railway Engineering Association - 1918 - 1644 páginas
...that specified in Section 13 (c) and any part of the fracture is more than 24 inch from the center of the gage length, as indicated by scribe scratches...specimen before testing, a retest shall be allowed. Requenchlng. 16. If the results of the physical tests of any test lot do not conform to the requirements...
Visualização integral - Acerca deste livro

Railroad Accident Report: Report no. NTSB-RAR.

United States. National Transportation Safety Board - 19?? - 678 páginas
...than that specified in Section 9 and any part of the fracture is more than 54 inch from the center of the gage length, as indicated by scribe scratches...specimen before testing, a retest shall be allowed. (d) No part of these specifications shall operate to cause any one tension test to apply to more than...
Visualização integral - Acerca deste livro

Bulletin, Volume 25,Parte 1

American Society for Testing Materials - 1925 - 978 páginas
...percentage of elongation of any tension test specimen is less than that specified in Section 7 (a) and any part of the fracture is outside the middle third of the gage length, as indicated by marks placed on the specimen before testing, a retest shall be allowed. IV. PERMISSIBLE VARIATIONS...
Visualização integral - Acerca deste livro

Industrial Standards, Volumes 1-30

United States. Bureau of Foreign and Domestic Commerce - 1918 - 730 páginas
...than that specified in section ю (a) and any part of the fracture is more than ^ inch from the center of the gage length, as indicated by scribe scratches marked on the specimen before testing, a re test shall be allowed. Retests. % 13. (a) If the results of the physical tests of any test-lot do...
Visualização integral - Acerca deste livro

Bulletin, Volume 24,Parte 1

American Society for Testing Materials - 1924 - 1192 páginas
...gage length of a 2-in. specimen or is outside the middle third of the gage length of an 8-in. specimen as indicated by scribe scratches marked on the specimen before testing, a retest shall be allowed." Table I. — Change the title to read as follows : "Permissible Variations of Rectangular Plates Ordered...