| American Railway Master Mechanics' Association - 1918 - 678 páginas
...(c) lf the percentage of elongation of any test specimen is less than that specified in Section 7, and any part of the fracture is outside the middle third of the gaged length, as indicated by the scribe scratches marked on the specimen before testing, a retest... | |
| American Society for Testing Materials - 1920 - 868 páginas
...the percentage of elongation of any tension test specimen is less than that specified in Section 5 and any part of the fracture is outside the middle...on the specimen before testing, a retest shall be allowedRetests. 9. If the results of the physical tests of any test lot do not conform to the requirements... | |
| Philippines - 2001 - 90 páginas
...substituted. C3.3 If any tensile property of any tension test specimen is less than that specified, and any part of the fracture is outside the middle third of the gauge length, as indicated by scribe scratches marked on the specimen before testing, a retest shall... | |
| George Bartholomew Haven, George Wright Swett - 1915 - 450 páginas
...percent age of elongat ion of any tension test specimen is less than that specified in Section 6 (a) and any part of the fracture is outside the middle...specimen before testing, a retest shall be allowed. 30 BOILERS AND PRESSURE VESSELS IV. PERMISSIBLE VARIATIONS IN GAGE. 9. The gage of each bar shall not... | |
| George Bartholomew Haven, George Wright Swett - 1915 - 470 páginas
...percentage of elongation of any tension test specimen is less than that specified in Section 6 (a) anil any part of the fracture is outside the middle third...specimen before testing, a retest shall be allowed. IV. PERMISSIBLE VARIATIONS IN WEIGHT AND GAGE. 12. When Ordered to Gage. — The thickness of each... | |
| American Society of Mechanical Engineers - 1915 - 1412 páginas
...percentage of elongation of any tension test specimen is less than that specified in Pars. 28 and 29, and any part of the fracture is outside the middle third of the gaged length, as indicated by the scribe scratches marked on the specimen before testing, a retest... | |
| American Society of Mechanical Engineers - 1915 - 1466 páginas
...percentage of elongation of any tension test specimen is less than that specified in Pars. 28 and 29, and any part of the fracture is outside the middle third of the gaged length, as indicated by the scribe scratches marked on the specimen before testing, a retest... | |
| Roy A. Seaton - 1916 - 246 páginas
...the percentage of elongation of any tension test specimen is less than that specified in Section 8(a) and any part of the fracture is outside the middle...specimen before testing, a retest shall be allowed. IV. PERMISSIBLE VARIATIONS IN WEIGHT 13. Permissible Variations. — The weight of any lot of bars... | |
| American Railway Master Mechanics' Association - 1916 - 1250 páginas
...elongation of any tension test specimen is less than that specified in Section 6 (a) and any part of thp fracture is outside the middle third of the gage length,...specimen before testing, a retest shall be allowed. IV. PERMISSIBLE VARIATIONS IN GAGE. 11. Permissible Variations. — The gage of each bar shall not... | |
| 1916 - 806 páginas
...percentage of elongation of any tension test specimen is less than that specified in Section 6 (a) and any part of the fracture is outside the middle...indicated by scribe scratches marked on the specimen bçforç testing, a retest shall be ajlowec}. — *^-^_ л n ( . AboutZ' . If. ' ""^ ' ,. . ! : ,.l... | |
| |